I am exited to try my new .8 nozzle. any suggestions on feeds, temp for ABS and PLA?
Date
Votes
2 comments
-
Mike Battaglia Hey Carlos, start with double the retraction distance, .3 coasting distance. Turn the heat up by 5 degrees: more material flowing means more heat loss, turning the heat up slightly will help compensate.
-
Shawn Fitzpatrick For what its worth, we had some discussion on this over here as well. We seemed to find that we needed to reduce the speed as otherwise we were pushing the plastic thru the hot end too fast and it couldn't actually maintain temperature.
We may have overlooked changing the coasting distance...